    The electrochemical behavior of Fe³⁺ – WO₄²⁻ – Cit³⁻ and Fe³⁺ – MoO₄²⁻ – WO₄²⁻ – Cit³ systems
    (Украинский государственный химико-технологический университет, 2017) Yermolenko, I. Yu.; Ved, M. V.; Karakurkchi, A. V.; Sakhnenko, N. D.; Kolupayeva, Z. I.
    The kinetic parameters of electrochemical behavior of tungsten at the deposition of Fe–W and Fe–Mo–W alloys were determined using linear voltammetry and analyzing polarization relationships. In the presence of citrate ions the cathode process was shown to proceed with the participation of [FeHCitWO₄]⁻ clusters. An optimal concentration ratio of the components in electrolyte required for the Fe—W alloy deposition was defined as c(Fe³⁺):c(Cit³⁻):c(WO₄²⁻) = 1:1.5:0.3. The deviation from this ratio by an increase in the concentration of tungstate ions results in the formation of dimer forms W₂O₇²⁻ and [FeW₂O₇HCit]⁻ clusters; as a result the concentration of electrode active particles [FeWO₄HCit]⁻ diminishes and the cathode process is inhibited. A peculiar feature of the formation of electrolytic alloy Fe–Mo–W is a competitive reduction of molybdates and tungstates. Based on the analysis of the kinetic parameters and characteristic criteria of electrochemical reactions, we proposed the mechanism for the co-deposition of alloy containing iron with molybdenum and tungsten; this mechanism is a sequence of coupled reactions of irreversible reduction of intermediates with slow charge transfer stage and previous chemical step of the ligands release. The data of X-ray phase analysis show that the binary alloys Fe–W are solid solutions of tungsten in iron and ternary alloys Fe-Mo- W are X-ray amorphous.
  • Ескіз
    Документ
    Functional properties of multicomponent galvanic alloys of iron with molybdenum and tungsten
    (Institute for Single Crystals, 2015) Karakurkchi, A. V.; Ved, M. V.; Sakhnenko, N. D.; Yermolenko, I. Yu.; Zyubanova, S. I.; Kolupayeva, Z. I.
    Galvanic alloy coatings Fe-Mo (W) and Fe-Mo-W were deposited from citrate bath based on Fe (III) using both direct and pulsed current on substrates steel 3 and grey cast iron GC 18. It was shown that the alloying components content, their distribution on the surface, morphology and topography of the coatings are depended on the electrolysis mode. It was established that the functional properties of the binary and ternary alloys of iron (corrosion resistance, microhardness, antifriction et al.) exceed parameters of the substrate and are predetermined by the composition, structure, material and surface roughness.